Purifying?agent?for?molten?zinc?in?HDG
Name:
Purifying?agent?for?molten?zinc?in?HDG
  • Model:
  • Uses:
  •  
Details

In the light of the high iron and impurity contents in molten zinc, poor fluidness and particles and fold on workpiece often occurred in hot galvanizing plants, our company has organized the famous specialists and scientific and technological personnel in many disciplines at home developed XY-XG-3 type purifying agent for molten zinc, a high and new technical product. It has effectively solved the difficult problem and filled in the gap in this field at home. Through testing and using, the agent reached the anticipated results and is well received by customers. At present the product is applying for a patent. 
Notice
Do well pretreatment work, do not carry the harmful impurity into zinc pot, galvanizing agent needs the acid and iron eliminating, and it would be best if rinsing water for pretreatment could be fluid.
Because of the high volatility of the agent, No.2 operation should be quickly performed.
In order to avoid the splashing of molten zinc causing danger, operators should be well dressed in labor protection articles. Operation with caution and safety first.
Purifying Treatment Method of Molten Zinc:
Keep furnace temperature at 450℃-470℃.
Place dry thermal insulation bricks (with strong water absorption) into box with holes, quickly pour the purifying agent to them, insert the box into molten zinc and move it back and forth until boiling ends, and take out the box with holes.
Eliminate suspended substances on the surface of molten zinc; scatter ammonium chloride (1-1.5 kg/ m2) to further eliminate impurity on the surface.
Repeat the abovementioned steps three or four times.
Add the alloy, which is 0.5% of molten zinc, in uniform distribution way. After all the melting, repeat the abovementioned step once. (If there are excessive aluminum or other alloys in original molten zinc, the step-by-step method can be used)
The temperature is controlled at 430℃-440℃ and the standing time is 6-12 h (time is as long as possible).
When small workpiece is tested (the temperature is at 430℃ and dipping time is not changed), the surface and coating thickness is measured. If the coating is thick, the alloy, which is 0.1 % of molten zinc, can be added. 
The zinc and the alloy can be added at one time until the alloy content in molten zinc reaches 1.5%.
After alloying is completed, the working temperature of molten zinc should be controlled at 440℃±5℃ and the lifting speed of traveling crane at 1.5 m / min.
 

 

返回頂部 電話
主站蜘蛛池模板: 欧美第一精品 | 成人永久免费视频 | www麻豆 | 香蕉av在线播放 | 一级成人免费视频 | 在线免费观看中文字幕 | 草在线视频 | 亚洲午夜激情视频 | 亚洲视频二 | 一级片久久 | 麻豆网址| 欧美在线91 | 国产精品久久久一区二区三区 | 中日韩欧美在线观看 | 国产一区免费看 | 黄色大片在线播放 | 性色av一区二区三区 | 国产成人亚洲欧洲在线 | 欧美色综合天天久久综合精品 | 日韩中文在线观看 | 日朝毛片 | 欧美一级免费 | 国产99精品视频 | 久久影片 | 99热免费在线观看 | 男人日女人网站 | 天堂а√在线中文在线鲁大师 | 中文字幕在线观看1 | 日韩毛片在线观看 | 国产精品国产三级国产aⅴ无密码 | 亚洲在线| 日本美女裸体视频 | 在线免费观看成年人视频 | 4虎影院在线观看 | 国产成人精品久久二区二区91 | 久久成人综合 | 在线看黄色网址 | 操亚洲女人 | 国产97在线视频 | 成人免费看片39 | 国产精久久久 |